Many assembly defects start long before a board reaches the reflow oven. Plastic IC packages soak up humidity from the air, bare boards do the same, and a single static spark can weaken a chip without leaving a visible mark. This guide explains moisture sensitivity levels, dry storage, baking, ESD control and part packaging in plain words — and shows how to prepare components you send us so your boards can be built without delays.

Get an instant quote

Two invisible risks before reflow: absorbed moisture and electrostatic discharge

Neither problem can be seen when you open a parcel of parts. Both can turn a correct design and a clean assembly into boards that fail in test — or worse, fail later in the field.

Absorbed moisture

Moulding compounds, die-attach materials and laminates are slightly porous and slowly take in water vapour. During reflow the package heats to well above the boiling point of water within a few minutes. Trapped moisture turns into steam, and the pressure can crack the package or separate internal layers (delamination). The extreme case makes an audible crack and is often called the “popcorn” effect.

Electrostatic discharge (ESD)

People, plastics and packaging build up static charge just by moving. A discharge into a pin can puncture thin gate oxides or melt tiny internal tracks. A person usually feels a spark only at a few thousand volts, while sensitive parts can be damaged by far less — so damage happens without anyone noticing.
Moisture damageESD damage
When it happensDuring reflow, wave soldering or rework heatingAny time a part is touched, moved, unpacked or placed
Typical resultPackage cracks, internal delamination, lifted bond wires, board blisteringImmediate failure, or a weakened part with higher leakage that fails later
Visible?Sometimes (bulging or cracks); often only with acoustic microscopy or X-rayAlmost never without electrical testing or failure analysis
Main preventionSealed dry packs, controlled floor life, dry storage, bakingGrounding, ESD-safe packaging, a controlled work area
Key standards (by name)J-STD-020, J-STD-033ANSI/ESD S20.20, IEC 61340-5-1

Moisture sensitivity levels (MSL 1–6) under J-STD-020 and what floor life means

Component makers test their plastic packages and give each one a moisture sensitivity level (MSL). The level tells you how long the part can sit in normal factory air after its sealed bag is opened before it must be soldered or dried again. That allowed time is called the floor life.

MSLTypical floor life after openingUsual packingWhat it means in practice
1Unlimited (at ≤30 °C / 85 % RH)Not required to be dry-packedNot moisture sensitive for normal reflow. Most passives and many simple packages.
2About 1 yearDry packLow risk; still keep sealed when not in use.
2aAbout 4 weeksDry packTrack the opening date; reseal leftovers.
3About 168 hours (one week)Dry packVery common for QFP, QFN, SOIC and many BGAs. Easy to exceed if a bag stays open on a bench.
4About 72 hoursDry packOpen only when the build is ready to start.
5About 48 hoursDry packNeeds planned handling and dry storage between uses.
5aAbout 24 hoursDry packEffectively a same-day part once opened.
6Time stated on the labelDry packMust be baked before use, then soldered within the label time.

Floor-life values are the commonly published figures for factory conditions of about 30 °C and 60 % relative humidity. The label on the actual bag is always the authority — it can differ by package, maker and peak reflow temperature.

Where to find the MSL

On the moisture-sensitive caution label of the sealed bag, in the datasheet (often under packaging or soldering information), or on the distributor’s product page.

The clock starts when the bag opens

Floor life counts the total time the parts spend outside dry conditions. Several short openings add up; they do not start fresh each time.

Higher reflow temperature, tighter rating

A package can carry a different MSL for lead-free (hotter) reflow than for leaded reflow. Check the rating that matches a lead-free profile if your assembly is RoHS.

Dry packs, humidity indicator cards and storage under J-STD-033

J-STD-033 describes how moisture-sensitive parts should be packed, stored, used and dried again. You do not need to read it to send parts safely — the basics below cover what matters.

Moisture barrier bag

A heat-sealed, metallised bag that blocks water vapour. Once it is cut open, it no longer protects the parts unless it is resealed with fresh desiccant.

Desiccant

Small pouches inside the bag that absorb remaining moisture. Desiccant has a limited capacity; old or saturated pouches do little.

Humidity indicator card (HIC)

A card with spots that change colour (commonly from blue to pink, or similar) at set humidity levels. It shows whether the air inside the bag stayed dry.

Caution label

Shows the MSL, the floor life, the bag seal date, the reflow peak temperature the rating applies to and the baking conditions. Keep this label with the parts — it is how anyone handling them knows the rules.

Sealed shelf life

A sealed dry pack is commonly rated for about 12 months from the seal date when stored below about 40 °C and 90 % RH. Older packs should be checked before use.

Dry cabinets

Cabinets held at very low humidity (typically 10 % RH or below, some at 5 % RH) keep opened parts dry between builds. Short exposures can often be offset by time in dry storage, as J-STD-033 describes.
  1. 1

    Open the bag only when you need the parts

    Cut close to the seal so the bag can be resealed. Note the date and time on the label.
  2. 2

    Read the humidity indicator card straight away

    If the card shows humidity above the level the label allows, assume the parts have absorbed moisture and need drying before reflow.
  3. 3

    Track exposure time

    Add up every period the parts are outside sealed or dry storage, and compare it with the floor life for their MSL.
  4. 4

    Reseal leftovers properly

    Put remaining parts back in a moisture barrier bag with fresh desiccant and a humidity card, then heat-seal or vacuum-seal it. A plain zip bag or tape is not a moisture barrier.

    Tip: Write the total exposure time used so far on the bag. The next person then knows how much floor life is left.

Baking parts that have been exposed too long: why it adds time and cost

Baking drives absorbed moisture out of a package so it can be reflowed safely. It works, but it is slow, it occupies oven capacity, and it is not free of side effects.

Method (general guidance)Typical conditionsTypical durationThings to know
High-temperature bakeAround 125 °CSeveral hours to about two days, depending on package thickness and MSLFastest method. Most tape, reels and tubes cannot survive this heat, so parts must be moved to heat-resistant trays.
Medium-temperature bakeAround 90 °C at ≤5 % RHFrom about a day to over a weekSome heat-rated carriers can stay in use; slower.
Low-temperature bakeAround 40 °C at ≤5 % RHDays to several weeks or longerGentle enough for most reels and tubes, but very slow.

Exact temperatures and times depend on the package body thickness and MSL and are listed in J-STD-033 and in the component maker’s instructions. Always follow those for the actual part.

Why baking adds time

Parts must often be moved out of reels into trays, baked for many hours, cooled, and then reloaded for placement. A part that arrives exposed can therefore delay the whole build by a day or more.

Why baking is not harmless

Heat speeds up oxidation of leads and growth of intermetallic layers on plated terminations, which can reduce solderability. Repeated or very long bakes should be avoided — this is why preventing exposure is better than fixing it.

Do not bake reels at high temperature

Most plastic carrier tape, reels and tubes soften or deform at oven temperatures used for fast baking, which can jam feeders or make the parts impossible to machine-place. If you think your parts need drying, tell us before you ship instead of baking them in their packaging yourself.

Bare PCBs absorb moisture too: delamination risk for boards stored a long time before assembly

FR-4 and other laminates take up moisture from humid air. During lead-free reflow the trapped water can expand and push the layers apart. IPC-1601 gives general guidance on handling and storing bare boards.

What can go wrong

Blisters between layers, measling (small white spots in the glass weave), inner-layer separation and damage around plated holes. Multilayer and thick boards are more exposed because moisture has further to travel out.

What raises the risk

Long storage in unsealed packaging, humid climates and monsoon seasons, several reflow passes (for example double-sided assembly), and rework heating.

How to reduce it

Keep boards in their sealed packing with desiccant until assembly, store them in a cool and dry place, and assemble them in a reasonable time after delivery.
Surface finishEffect of storage timeBaking note (general guidance)
HASL / Lead-free HASLStores well when sealedCan usually be baked if needed
ENIGStores well when sealedCan usually be baked if needed
OSPShortest shelf life; the protective film degrades with time and heatHot baking can damage the OSP film and reduce solderability — plan assembly soon after delivery instead

Ordering both boards and assembly from Microplacer

Ordering bare boards and assembly together helps avoid a long storage gap between fabrication and assembly. If you send boards made elsewhere, tell us how old they are and how they were stored. Read more about finishes and shelf life in choosing a surface finish.

ESD-sensitive parts and the basic controls behind ANSI/ESD S20.20

ANSI/ESD S20.20 (and its international counterpart IEC 61340-5-1) describes how to set up an ESD control programme. The idea is simple: keep everything at the same potential, and keep charges away from sensitive parts.

ControlWhat it does
Grounded wrist straps and footwearDrain the charge from people before they touch parts or boards.
Dissipative work surfaces and flooringLet charge flow away slowly and safely instead of in a sudden spark.
ESD protected area (EPA)A marked zone where only ESD-safe materials and trained, grounded people handle unprotected parts.
IonisersNeutralise charge on insulating items, such as plastic housings, that cannot be grounded.
Shielding packagingMetallised shielding bags form a cage around the contents, so external fields and sparks do not reach the parts.
Training and checksRegular testing of straps, surfaces and grounding points, and training for everyone who handles parts.
Packaging typeProtects againstSuitable for shipping sensitive parts?
Metallised static-shielding bagCharge build-up and external dischargeYes — the usual choice for loose ICs, modules and assembled boards
Moisture barrier bag (dry pack)Moisture; most are also static-shieldingYes — for moisture-sensitive parts
Pink or coloured “antistatic” bagCharge build-up on the bag itself onlyNot on its own — it does not shield from outside discharge
Black conductive foamKeeps all leads at the same potentialYes for leaded parts, inside a shielding bag
Ordinary plastic bag, bubble wrap or foamNothing — these can generate chargeNo

Which parts are ESD sensitive?

Treat every semiconductor as ESD sensitive: microcontrollers, MOSFETs, RF parts, sensors, LEDs and laser diodes, and many ICs with very small geometries are especially vulnerable. Device sensitivity is classified with test models such as the human body model (HBM) and charged device model (CDM); the datasheet often lists the rating.

Packaging for consigned parts: reels, cut tape, tubes and trays, and what can be machine-placed

Placement machines pick parts from feeders. How a part is packed decides whether it can be fed automatically, needs special handling, or cannot be machine-placed at all.

PackagingMachine placementGood practice when sending
Full reelBest — loads straight onto a feederKeep the reel label visible and the tape end secured.
Cut tapeUsually possibleSend one continuous strip per part, not many short pieces. Leave extra empty pockets at the start so the tape can be threaded into a feeder.
TubeUsually possible for SOIC, DIP and similarKeep end stoppers in place so parts cannot slide out; keep all parts facing the same way.
Tray (matrix tray)Usually possible for QFP, BGA and large ICsCover and strap the tray so parts cannot jump pockets; keep pin 1 orientation consistent.
Loose parts in a bagUsually not possible for small SMD partsAvoid for SMD. Loose fine-pitch or tiny parts risk bent leads, mixed values and lost orientation.

Label every package

Mark each reel, strip, tube or tray with the manufacturer part number and the BOM designators it is for. Unlabelled passives cannot be identified by eye.

Keep the original packaging

Original sealed dry packs and shielding bags carry the MSL label, date codes and traceability. Repacking loses that information.

Tell us about special parts

Packages such as BGA, LGA and 0201 go to engineering review in our assembly quote. If you supply them, mention it so handling is planned. See design for assembly.

Extra parts (overage) to cover machine losses when you supply your own components

Automatic placement always uses a few more parts than the BOM count. Some are used when a feeder is set up, and occasionally a machine drops or rejects a part. Without spares, a single lost part can stop a build.

Part type (general rule of thumb)Typical extra to sendWhy
Small passives (0402, 0603) on tapeA few percent extra, plus a fixed number of spares per lineTiny parts are most often dropped; setup uses some of the tape.
Larger passives and discretes on tapeA smaller percentage extraLower loss rate, but setup still uses some parts.
ICs in tape, tubes or traysOne or two spares per part number where possibleLosses are rare, but a single shortage blocks every board.
Expensive or hard-to-find partsDiscuss with us before shippingWe can plan careful handling instead of large overage.
Cut tapeExtra length at the start of each stripEmpty and first pockets are used to thread the feeder.

These are common industry rules of thumb, not fixed figures. We confirm exactly what to send for your order after checking your BOM.

What to send us and what to specify when ordering

Clear information up front avoids the most common delays with customer-supplied parts: unidentified reels, exposed moisture-sensitive parts and short quantities.

InformationWhy we need it
BOM with manufacturer part numbers and designatorsLets us match every package to its positions on the board. Components are quoted from the BOM.
Which parts you will supply and which we sourceChoose “I will supply” or “Some by me” in the calculator, so the quote only includes the parts we buy.
MSL of moisture-sensitive partsLets us plan handling and the order of work around the floor life.
Opening history of any previously opened dry packsTells us how much floor life is left, or whether drying is needed first.
Packaging type and quantity per partLets us check machine placement and overage before the parts arrive.
Production notes in your filesOur engineers read notes in your files and compare them with our options before production.

How this fits into ordering at Microplacer

The PCBA instant price is calculated from solder pads; for 5–50 boards the stencil is free and for 55 or more a shared stencil is used. Assembly is done in panels only. Packages such as BGA, LGA and 0201 are sent to engineering review. Parts we source are quoted from your BOM, and you can also buy from our components store with millions of parts — see electronic components. Our engineers check your files before production.

Checklist for shipping components to us

Follow these steps for any parts you send for assembly.

  1. 1

    Place your order and confirm the parts list

    Mark which parts you will supply in the calculator. We confirm exactly what to send after checking your BOM — see the assembly quote FAQ.
  2. 2

    Keep moisture-sensitive parts sealed

    Ship MSL 2a and higher parts in their original unopened dry pack where possible. If a pack has been opened, reseal it with fresh desiccant and a humidity card and note the exposure time used.
  3. 3

    Use ESD-safe packaging for all semiconductors

    Metallised shielding bags or the original sealed packs. Do not use ordinary plastic bags, bubble wrap or foam directly against parts.
  4. 4

    Keep parts machine-placeable

    Send reels, continuous cut tape with extra leading pockets, capped tubes or covered trays. Avoid loose SMD parts.
  5. 5

    Add overage

    Include spares as described above, especially for small passives.
  6. 6

    Label everything

    Each package should show the manufacturer part number and the BOM designators. Add a packing list with your order reference inside the box.
  7. 7

    Pack the parcel securely

    Use a rigid box with padding around the bags, so reels cannot bend and trays cannot open in transit.
  8. 8

    Tell us before you ship

    Let us know when the parcel is on its way so we can match it to your order. See also the guidance on consigned parts on the electronic components page.

    Tip: If any part is missing or short, tell us early. We can check whether it is available in our components store so the build is not held up.

Frequently asked questions

Look at the caution label on the sealed bag, the packaging or soldering section of the datasheet, or the distributor’s product page. If a part has no MSL and is not dry-packed, it is usually MSL 1.

A short opening uses only a little floor life. Reseal the bag with fresh desiccant and a humidity card as soon as possible, and tell us roughly how long it was open.

We suggest you do not. Most reels and tubes cannot take high-temperature baking, and repeated baking can reduce solderability. Tell us about the exposure instead so we can advise how to handle the parts before the build.

They stop the bag itself from charging up, but they do not shield the contents from outside discharge. For ICs and other semiconductors, metallised static-shielding bags or the original sealed packs are the safer choice.

Short pieces and loose SMD parts are hard or impossible to feed into placement machines. Send one continuous strip per part with extra leading pockets. If you only have loose parts, contact us before shipping.

As a general rule, a few percent extra for small passives and a spare or two for ICs where possible. We confirm exactly what to send after checking your BOM.

Keep them sealed with desiccant in a cool, dry place and assemble them in a reasonable time. Boards with an OSP finish have the shortest shelf life. Ordering boards and assembly together avoids a long storage gap.

Related guides

Still have a question?

Send us your files or call us — our engineers will help you choose the right options for your boards and assembly.

Streamline your innovation with seamless PCB ordering.

For More Details Contact Us